• Temperature-Salt-Resisting Polyacrylamide for Oil Drilling
  • Temperature-Salt-Resisting Polyacrylamide for Oil Drilling
  • Temperature-Salt-Resisting Polyacrylamide for Oil Drilling
  • Temperature-Salt-Resisting Polyacrylamide for Oil Drilling
  • Temperature-Salt-Resisting Polyacrylamide for Oil Drilling
  • Temperature-Salt-Resisting Polyacrylamide for Oil Drilling

Temperature-Salt-Resisting Polyacrylamide for Oil Drilling

Certification: ISO 9001
Environmental Protection: Yes
Color: White
Appearance: Granulars
Kind: Mud Additives
Application: Lubricant Additives
Samples:
US$ 1/Piece 1 Piece(Min.Order)
| Request Sample
Customization:
Diamond Member Since 2007

Suppliers with verified business licenses

Manufacturer/Factory & Trading Company

Basic Info.

Model NO.
TRS-PAM
CAS
9003-05-8
Viscosity
Low - Higher
Molecular Weight
Low - Very Higher
Charge Density
10% - 40%
Transport Package
25kg plastic enhanced paper bag
Specification
ISO
Trademark
bluwat
Origin
china
HS Code
39140000
Production Capacity
1000mt per month

Product Description

Temperature-salt-resisting Polyacrylamide
Brief introduction
Temperature-salt-resisting Polyacrylamide is developed for the sewage in EOR (Enhanced oil recovery), it can help use sewage recycle and protect environment. It is mainly used in oil field with high salt and temperature.

Advantage:
1. Anti-temperature
2. Anti-salt
3. Low dosage, higher performance

Uses
Used as oil displacement agent in the oil field with high temperature and mineralization degree

Packing & storage
25kg paper-plastic composite bag, or following your demand. Its powder can adsorb the moisture and become the block matter, thus it should be kept in dry, cool and ventilating place.
Technical index
 
BWEOR-1
 
BWEOR-2
 
BWEOR-3
 
Granularity (mesh)
 
                          20-80
 
Solid (%)
 
                         ≥ 89
 
Dissolved time(h)
 
                        ≤2
 
Insoluble matter (%)
 
                        ≤0.2
 
Molecular weight(106)
 
≥2000
 
≥2500
 
≥3500
 
Degree of hydrolysis (%)
 
                         23-27
 
Residual monomer (%)
 
                        ≤0.1
 
filtration ratio
 
                        ≤2.0
 
Apparent Viscosity (mpa . s)
   Concentration (1500mg/L)
degree of mineralization (19334mg/L)
     Temp.( 75 )
 
    ≥11.5
 
    ≥12.5
 
    ≥12.5
 
Apparent Viscosity (mpa.s)
   Concentration (1000mg/L)
degree of mineralization (2500mg/L)
   Temp.( 45 )
 
    ≥40
 
    ≥45
 
    ≥50
 
Retention rate of shearing Viscosity (%)
 
                        ≥80
 
Retention rate of static adsorption Viscosity (%)
 
                        ≥80
 
Temperature-Salt-Resisting Polyacrylamide for Oil Drilling
Temperature-Salt-Resisting Polyacrylamide for Oil Drilling
Temperature-Salt-Resisting Polyacrylamide for Oil Drilling
Temperature-Salt-Resisting Polyacrylamide for Oil Drilling
 

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now

You Might Also Like

Diamond Member Since 2007

Suppliers with verified business licenses

Manufacturer/Factory & Trading Company
Year of Establishment
2004-01-02
Management System Certification
ISO 9001